Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Mapex" in Material Data Center leads to the following information:

Tradename: Mapex
Family: PA6, PA66, PA666
Producer: Ginar Technology Co.,Ltd
58 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Market News
...an for the European market, with immediate effect. Ginar claims to be one of the biggest Taiwanese compounders with production sites in Taiwan and China. Through this cooperation, Clickplastics has extended its product range by Aplax PP compounds, Mapex PA6/66 compounds and Kapex PC compounds. The Ginar Technology Co. Ltd. products already have approvals for the Asian automotive, electrical engineering and electronic industries and can thus also be introduced on to the European market relatively...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.