Mirel - PHA - Telles
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Mirel" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
As part of the commercialization process for Mirel PHA bioplastics, it became necessary to validate the injection molding process for a high-profile consumer products launch. Since Mirel is a new poly...
Kunststoffe international, 2007-10-21, Bioplastics
...s and carrier bags made from its novel starch blends, is also penetrating into Europe. The compounder FKuR has doubled its processing capacity for the production of mixtures of PLA with other polyesters to 7,000t/a. Mirel, a joint venture of the US company Metabolix and Archer Daniels Midland (ADM), is currently building a 50,000t plant for the PHA polyester, produced by bacteria from sugar. It is planned to come on stream next year. After a successful IPO, Plantic of Australia has invested subs...
Kunststoffe international, 2008-08-14, Bio – What Else?
...Ingeo to make it easier to differentiate between the company and its product. Telles, the manufacturer of raw biopolymers, is a joint venture between Metabolix Inc. and Archer Daniels Midland (ADM). It manufactures Mirel, a polyhydroxyalkanoate (PHA). PHA is obtained with the aid of bacteria from corn sugar and other renewable raw materials. Tianan Biologic calls itself the world’s largest producer of PHBV, a valerate of PHA. Its current production capacity will double this year,...
Kunststoffe international, 2011-10-17, Bioplastics
...off GmbH, of Höxter, Germany, or Victor Güthoff & Partner GmbH of Frechen, Germany, have successfully specialized in biobags. Starch materials are not the only ones used. Mirel-PHA types suitable for films also became available recently. Even relatively brittle PLA can be used to produce carrier bags by compounding it appropriately. Cerestar of El Segundo, USA, announced in May that it would set up the production of starch materials in Assisi, Italy. Bio-based polyolefins and PET: The curren...
Kunststoffe international, 2014-08-19, Sustainable Solution for Coloration of Bioplastics
.... Formulations specially tailored to customer requirements are also possible. Temperature tests have shown a heat resistance of up to 150 °C for 5 min, which is sufficient for film extrusion of bioplastics from the PHA family (e. g. Mirel from Metabolix Inc., Cambridge, MA/USA) to produce items such as disposable or multi-trip plastic bags (Fig. 2). However, this colorant class cannot withstand the processing temperatures in masterbatch production (about 200 °C and more).At Low TemperaturesThe b...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.