Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Peek-Classix" in Material Data Center leads to the following information:

Tradename: Peek-Classix
Family: PEEK
Producer: Invibio Inc
3 hits in the literature database
1 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Europe is the Largest Market: Polyaryletherketones (PAEK)
...of extractables. Ultra-High-Purity PEEK contains no additives, fillers or stabilisers that could leach out in liquids or outgas in a vacuum. Invibio, the wholly owned subsidiary of Victrex plc., has developed a new biocompatible product known as PEEK-Classix for medical applications involving less than 30 days blood contact. This new PEEK fills a gap between the PEEK-Optima grades for long-term implants and the Victrex PEEK engineering grades Strategic Market Development and New Applications ...

Kunststoffe international, 2005-11-21, High-performance Polymers: Metal Substitution and Miniaturisation
Trade Fair Report Metal Substitution and Miniaturisation High-performance Polymers. Fuel cells, short-term implants, miniaturised electronic components and even baking moulds – high-performance plastics are to be found almost everywhere. Designers always choose members of this small group of specialty polymers for parts that require high thermal stability or special properties such as chemical resistance, high light transmission or biocompatibility. Visitors to K2004 were able to discover numer...

Kunststoffe international, 2007-10-21, Polyaryletherketones (PAEK)
Polyaryletherketones (PAEK) Increasing Demand (Trade-fair-pre-report K 2007) Worldwide demand for PAEK continues to increase at an annual rate of approx. 15%. In addition to Victrex, the world’s largest producer of PAEK, two new suppliers, Degussa and Solvay, have appeared on the scene to develop additional applications. Wolfgang Reimer and Horst Sandner Back in 1981, British ICI launched two linear aromatic semi-crystalline thermoplastics, polyetheretherketone (PEEK) and polyetherketone (...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.