Printex - Colorants, Fillers, UV-light stabilizers - Orion Engineered Carbons GmbH

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Printex" in Material Data Center leads to the following information:

Tradename: Printex
Family: Colorants, Fillers, UV-light stabilizers
Producer: Orion Engineered Carbons GmbH
2 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Barely Affected
...glass fibres. The graph for PA 6 pigmented with phthalocyanine green shows the same viscosity characteristics as the blue and has therefore not been included here. Carbon black The results obtained when pigmenting with carbon black (furnace black, Printex 80) are very surprising indeed (Fig. 4A). Although it is said that carbon black exerts a major influence - for example in injection moulding - this is not actually reflected in the viscosity data. Particularly in the range of high shear rates,...

Kunststoffe international, 2005-11-21, Market and Trends: Nanomaterials: Opportunities and Risks
...ack with nanostructured surfaces decreases the rolling resistance of tires, can saving up to 5% fuel and increases the life expectancy of tires. Electrically conducting carbon black (grade: Printex XE, manufacturer: Degussa) consists of carbon nanoparticles approximately 20nm in diameter. Via nanoparticle percolation plastics become electrically conducting at even less than 5wt.-%, and can be rendered antistatic or shielded against electromagnetic radiation. Today new molecular forms of carbon a...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.