Radel - PPSU - Solvay Specialty Polymers
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Radel" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...d from this are mounted on the wing leading edges and are about 20% lighter than the aluminium part used until now, which saves fuel costs. Also on board, in the form of transparent partitions between the different seating categories, is Radel R 7000 tr from Solvay. Polyphenylsulphone’s premiere in the Airbus was expedited by its high transparency, notch impact resistance and low environmental stress cracking. With a glass transition temperature of 265°C and a heat deflection temperature of 255...
Kunststoffe international, 2005-11-21, Impressive Variety: Polysulfones (PSU, PESU, PPSU)
...one polymers are available on the market: polysulfone (PSU), polyethersulfone (PESU) and polyphenylsulfone (PPSU). In addition, polysulfone blends have also appeared in a number of marketable products. Sulfone Polymers Performance With Udel (PSU), Radel A (PESU) and Radel R (PPSU), Solvay Advanced Polymers covers all three product areas. Polysulfone blends are available under the trade name Mindel. Compared to using pure PSU, these blends of PSU and engineering thermoplastics with moderately he...
Kunststoffe international, 2005-11-21, Sulfone Polymers: Sound Properties
...olyphenylsulfone (PPSU) in particular is a material of choice, since with steam sterilisation temperatures of 134°C must be tolerated for 18min a thousand times or more. Thanks to its thermal properties, this poses no problem for the PPSU grade Radel R from Solvay Advanced Polymers, which has a glass transition temperature of 220°C and an exceptional heat distortion temperature (HDT) A-value of 207°C. However, other criteria must also be met. For instance, the mechanical properties – above all, ...
Kunststoffe international, 2005-11-21, Sulphone Polymers: Clear Vision
...Transparent and Heat Resistant Sulphone polymers, as amorphous materials, are inherently transparent. The Solvay Advanced Polymers range of HT thermoplastics includes three transparent products: PSU, with the trade name Udel; PES with the trade name Radel A, and PPSU with the trade name Radel R. In addition to their good optical properties, sulphone polymers have the highest heat distortion temperature (HDT. Udel PSU has an HDT of 174°C, while Radel A PES and Radel R PPSU have values of 204°C an...
Kunststoffe international, 2008-04-14, Streets ahead of Injection Molding
...ring plastics (including ionomer, POM, PBT, PC, PMMA, PA6 and PA66), as well as in a thermoplastic polyurethane elastomer (TPU). Tests with the high-performance plastics PEI (grade: Ultem; manufacturer: Sabic Innovative Plastics), PPSU (grade: Radel R; manufacturer: Solvay GmbH) and PEEK (grade: Victrex PEEK; manufacturer: Victrex plc) produced strips in a quality that cannot be attained through the conventional form of production by injection molding or extrusion. A large number of special inje...
Kunststoffe international, 2008-10-17, Polyarylsulfones (PSU, PESU, PPSU)
...solely by Sabic. In 2006, Solvay, too, launched new, directly metallizable polyethersulfones for the lighting sector. They are designed for operating temperatures of up to 205°C and are notable for their high melt flow rates (Radel LTG-3000 PES). In particular, it is difficult to realize new ideas such as cornering lights or highly stylized daytime running lights without PESU or PEI due to the high demands on the geometry. Free-flowing polysulfones, such as Udel LTG-2000 (manufacture...
Kunststoffe international, 2011-10-17, Polyarylsulfones (PSU, PESU, PPSU)
...SU offer a more constant range of properties under changing temperatures. Manufacturers, Capacities, Production After the takeover of Gharda by Solvay in 2006, and the subsequent portfolio optimization, with substitution of the Gafone brands with Veradel brands, there are still three large producers of polyarylsulfones in the world: BASF SE, Ludwigshafen, Germany, Solvay, Brussels, Belgium, and Sumitomo, Sendai, Japan. The associated production capacity increased by more than 30 % in the past fi...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.