Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Ramofin - PP - Polyram

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Ramofin" in Material Data Center leads to the following information:

Tradename: Ramofin
Family: PP
Producer: Polyram
128 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
RamOfin PPH106 PP
RamOfin PL103BL18 (PE-HD)
RamOfin PL300S4BK10 PE-GB20
RamOfin PL305C6 PE-Z30
RamOfin PL306G4NT PE-GF20
RamOfin PL330G8NT PE-GF40
RamOfin PL4001NT (PE+PTFE)
RamOfin PPC100BK10 PP
RamOfin PPC101BK11 PP
RamOfin PPC103BK11 PP
RamOfin PPC108WT41 PP
RamOfin PPC300S4NT PP-GB20
RamOfin PPC301G2BK11 PP-GF10
RamOfin PPC301G2NT PP-GF10
RamOfin PPC301R05 PP-CF5
RamOfin PPC302G6BK10 PP-GF30
RamOfin PPC302G6NT PP-GF30
RamOfin PPC307G2BK11 PP-GF10
RamOfin PPC311J4BK11 PP-(GF+GB)20
RamOfin PPC341T4NT PP-T20
RamOfin PPC344T4NT PP-T20
RamOfin PPC345T4BK11 PP-T20
RamOfin PPC346T5NT PP-T25
RamOfin PPC350M6BK11 PP-MX30
RamOfin PPC359T4NT PP-MX20
RamOfin PPC371B73BK10 PP-MX73
RamOfin PPC371B73NT PP-MX70
RamOfin PPC372B73NT PP-MX73
RamOfin PPC500BK10 PP
RamOfin PPC500BL56 PP
RamOfin PPC500OR11 PP
RamOfin PPC501BK10 PP
RamOfin PPC501G6GR225 PP-GF30
RamOfin PPC501NT PP
RamOfin PPC502NT PP
RamOfin PPC507GR71 PP
RamOfin PPC571NT PP
RamOfin PPC571WT244 PP
RamOfin PPC702G3BK11 PP-GF15
RamOfin PPC705BK11 PP
RamOfin PPC705BK11H PP
RamOfin PPC5002T4BK10 PP-T20
RamOfin PPC5002T4GR153 PP-T20
RamOfin PPC5002T4NT PP-T20
RamOfin PPC5002T4WT36 PP-T20
RamOfin PPC5003T5GR430 PP-T25
RamOfin PPC5003T5NT PP-T25
RamOfin PPC7001G6BK11 PP-GF30
RamOfin PPC8001G6NT PP-GF30
RamOfin PPH203G5NT PP-GF25
RamOfin PPH203G50NT PP-GF50
RamOfin PPH300G4BK10 PP-GF20
RamOfin PPH300G4BK11 PP-GF20
RamOfin PPH300G4GR327 PP-GF20
RamOfin PPH300G4NT PP-GF20
RamOfin PPH300G4NTA PP-GF20
RamOfin PPH300G4WT49 PP-GF20
RamOfin PPH300G6BK10 PP-GF30
RamOfin PPH300G6BK10-M PP-GF30
RamOfin PPH300G6BK10-Z PP-GF30
RamOfin PPH300G6BK11 PP-GF30
RamOfin PPH300G6BK11-PW PP-GF30
RamOfin PPH300G6BK11Z PP-GF30
RamOfin PPH300G6BL209 PP-GF30
RamOfin PPH300G6GR162 PP-GF30
RamOfin PPH300G6NT PP-GF30
RamOfin PPH300G6NTA PP-GF30
RamOfin PPH300G6WT136 PP-GF30
RamOfin PPH300G8BK10-Z PP-GF40
RamOfin PPH300J8BK10 PP-(GF+GB)40
RamOfin PPH300J8NT PP-(GF+GB)40
RamOfin PPH300J8WT54 PP-(GF+GB)40
RamOfin PPH300S2BK10 PP-GB10
RamOfin PPH300S2BL195 PP-GB10
RamOfin PPH300S2OR56 PP-GB10
RamOfin PPH301G6NT PP-GF30
RamOfin PPH302G4GN56-1 PP-GF20
RamOfin PPH303G6NT PP-GF30
RamOfin PPH304G2BK11-IM PP-GF10
RamOfin PPH304G2NT PP-GF10
RamOfin PPH305G6BK11 PP-GF30
RamOfin PPH306G6BK10 PP-GF30
RamOfin PPH306S6BK10 PP-GB30
RamOfin PPH307G6BK10 PP-GF30
RamOfin PPH308G6BK11 PP-GF30
RamOfin PPH308G8BK11 PP-GF40
RamOfin PPH308G8BK11-I PP-GF40
RamOfin PPH308G8GN56 PP-GF40
RamOfin PPH308G8GR28 PP-GF40
RamOfin PPH308G50BK11 PP-GF50
RamOfin PPH309G6BK11 (PP+PTFE)-GF30
RamOfin PPH310G4NT PP-GF20
RamOfin PPH310G6NT PP-GF30
RamOfin PPH310G6OR51-2 PP-GF30
RamOfin PPH310G8NT PP-GF40
RamOfin PPH313G6NT PP-GF30
RamOfin PPH317G4GR406 PP-GF20
RamOfin PPH331G4NT PP-GF20
RamOfin PPH339G8BK10 PP-GF40
RamOfin PPH342T4NT PP-T20
RamOfin PPH343T4BK10-1 PP-T20
RamOfin PPH343T8NT PP-T40
RamOfin PPH346T4BK11 PP-T20
RamOfin PPH354T8NT PP-T40
RamOfin PPH356G8GR28 PP-GF40
RamOfin PPH380G50BK10 PP-GF50
RamOfin PPH380G50NT PP-GF50
RamOfin PPH501G4BK10 PP-GF20
RamOfin PPH501G4WT222 PP-GF20
RamOfin PPH502G4BK10 PP-GF20
RamOfin PPH503BK10 PP
RamOfin PPH505BK10 PP
RamOfin PPH505CR67 PP
RamOfin PPH505GR62 PP
RamOfin PPH505GR87 PP
RamOfin PPH505WT55 PP
RamOfin PPH570G6BK11 PP-GF30
RamOfin PPH703G2BL109 PP-GF10
RamOfin PPH3001G4BL151 PP-GF20
RamOfin PPH3001G6BL151 PP-GF30
RamOfin PPH3001G50BK11 PP-GF50
RamOfin PPH3401S50NT PP-GB50
RamOfin PPH3402J43BK54 PP-(GF+GB)43
RamOfin PPH7001G6GR417 PP-GF30
RamOfin PPH7002G4RD100 PP-GF20
RamOfin RPPH301G6BK10 PP-GF30
RamOfin+ PPH300G4NT BIO PP-GF20
RamOfin+ PPH300G6NT BIO PP-GF30

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.