Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Rilsan - PA11, PA12 - ARKEMA

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Rilsan" in Material Data Center leads to the following information:

Tradename: Rilsan
Family: PA11, PA12
Producer: ARKEMA
73 hits in the material database
6 hits in the literature database
4 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Lignin - Tailor-made
...wly Polyamide 11 lignin compounds were produced on a Werner and Pfleiderer ZSK 25 laboratory extruder with an L/D ratio of 42 at 200°C. The residence time was about 60 s at an output of 5 kg/h and a speed of 200 rpm. The polyamide used was Rilsan B MF20 from Atofina, while the lignin was abaca granite lignin (see Table 1). In Figures 2 and 3, the mechanical properties of polyamide 11 (Tm = 185°C) compounds are plotted against the lignin content (abaca lignin, Tm = 150°C). Significan...

Kunststoffe international, 2008-01-15, Elastomer Industry Has Understood
...c elastomers (Pebax Rnew) with a 20 to 90% renewable carbon content. Arkema has been a global market leader in C11-w-amino acid chemistry for 60 years and uses a unique chemical of vegetable origin – castor oil – to produce Rilsan PA11 (Fig.1). This natural vegetable oil is obtained from an inedible and non-genetically modified useful plant and therefore is not in competition with food production. The use of castor-oil-based raw materials in this product range reduces demand for fossil energy an...

Kunststoffe international, 2010-09-24, Systematic Metal Substitution
The polyphthalamide Rilsan HT is a new member of the polyamide 11 (Rilsan PA11) and polyamide 12 (Rilsan PA12) family of engineering polymers from Arkema. Polyamide 11, which is derived 100 % from renewable vegetable feedstock (or oil), and polyamide 12 have been used for decades as a metal substitute in the automotive industry. Rilsan PA11 is already established for flexible high-temperature applications, such as biodiesel fuel lines or brake booster tubing, up to150°C. In order to extend metal...

Kunststoffe international, 2011-04-25, Flame Retardants: Restricted Boom
...e polymers that are partly or wholly produced from renewable raw materials and biodegradable. At K2010, different polymer producers showcased new developments in polyamides based on or oil (Fig. 5). Important producers include Arkema (Rilsan, PA11), BASF (Ultramid Balance, PA610), DSM (EcoPaXX, PA410), DuPont (Zytel RS, PA610 and PA1010) and Evonik (Vestamid Terra DS, PA1010). While most polyamides based on or oil are used in applications without flame retardancy requirements, DSM Engineering Pl...

Kunststoffe international, 2011-10-17, Polyamides (PA)
... 2). Suppliers of special polyamides have added partly aromatic products to their range of PA products too, for instance Evonik Industries AG in Marl, Germany, (Vestamid HT) and Arkema SA in Colombes, France, offering the flexible Rilsan HT designed for fuel systems. With an increasing number of vehicles using Adblue, which is an aggressive urea solution employed to reduce NOx emissions, special polyamides with corresponding properties have recently been introduced for pumps, dosing units or fil...

Kunststoffe international, 2017-02-23, Organoclay Imparts Scratch Resistance
... Further studies with the addition of thermal stabilizers should thus be carried out. WMaterialTrade name and descriptionManufacturerPMMAPlexiglas V825Arkema PA6Akulon K222-DDSM Engineering PlasticsPA6Nycoa 1637NycoaPA12Grilamid TR90EMS-GrivoryPA12Rilsan AMNOArkemaPCLupoy PC 1201-22LG ChemOrganically modified organoclayCloisite 11: natural bentonite, modified with benzyl, hydrogenated tallow and dimethylammonium chlorideBYK Additives Cloisite 30B: natural montmorillonite, modified with methyl, t...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.