Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Santoprene" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
... designed, integrated elastomer elements (soft component). The centre part shown in Fig.2 for the Audi A4 from 1994 was manufactured by two-component injection moulding by the transfer technique. The mechanically coupled soft component was made of a Santoprene TPE. Because of the narrow manufacturing and assembly tolerances, the hard component was a PPO (grade: Noryl), which, as an amorphous thermoplastic, has uniform solidification behaviour and therefore low warpage. The thermal and mechanical...
Kunststoffe international, 2005-11-21, Rugged and Impact-resistant
...plastic elastomer. The firm CD3 Storage Systems Inc. based in Texas, USA, has developed a particularly rugged, portable storage box for CDs. The housing of the new Discus range of boxes is made of a crosslinked thermoplastic elastomer (TPV; grade: Santoprene 8000, manufacturer: Advanced Elastomer Systems; AES). The designer used a polypropylene for the closure and the decorative graphics. This combination of materials provides good mechanical protection and also has an impact-absorbing effect....
Kunststoffe international, 2005-11-21, Thermoplastic Elastomers (TPE)
...ed with hot-transfer decorative film and coloured with masterbatches. The robust housing of the portable computer for outdoor use shown in Fig.8 is made of a (PC+ABS) blend. The edge protection applied by two-component injection moulding is in Santoprene TPE-V from Advanced Elastomer Systems NV/SA (AES), Brussels/Belgium, which means that the computer will withstand being dropped from a height of 1.5m without suffering any damage. Because of its good compatibility with different plastics, this m...
Kunststoffe international, 2005-11-21, Tools: A Better Grip
...bility in design – improved ergonomics and appearance through easy colourability and problem-free adhesion to other materials, plus, - simple processing by injection moulding. Good Adhesion to Rigid Substrates Thermoplastic vulcanisates in the Santoprene product range supplied by AES, Brussels/Belgium, have a pleasantly soft touch and bond to a large number of substrates, including PP, PA, ABS, PC, PS, ASA, PMMA, PET, PPO and PBT, as well as to corresponding material mixtures. The TPV grades i...
Kunststoffe international, 2005-11-21, Walking Aids in TPV: Lightweight and Stable
...nsured by the use of material combinations which offer comfort, strength and stability. Brown's device comprises an extruded aluminium shaft, some 1.30m in length, with a honeycomb core. The soft grips on the stand-up and walking aid are made of Santoprene thermoplastic vulcanisate (TPV), manufactured by Advanced Elastomer Systems, a subsidiary of ExxonMobil Chemical. At the bottom of the shaft is the anchor pad, a rectangular foot made of Vyram thermoplastic elastomer. These two rubber-like...
Kunststoffe international, 2006-01-15, Process Development: Tomorrow’s Tubes Today
...its licensees with regard to in-situ technical support and polymer supply chain management, polymer quality and consistency, Zestron formed a strategic alliance with - raw material manufacturer ExxonMobil Chemical (www.santoprene.de) - toolmakers Otto Hofstetter AG (www.otto-hofstetter.ch) and - automation specialist Waldorf Technik GmbH & Co KG (www.waldorf-technik.de) Zestron alone is responsible for granting production licences. According to Ian Jacobs many companies from the packaging in...
Kunststoffe international, 2007-09-19, Plastics and Robotics Take Off
...the flexible extrusion of different sealing profiles directly onto the part by a six-axis RV30-26 industrial robot (Fig.1). The advantages of this application are customization of the sealing profile (Fig.2) with almost loss-free recycling of the Santoprene sealing material, and immediate availability of the part. In conjunction with PP, the sealing material is 100% recyclable. At the same time, the company presents its new subsidiary Reis Extrusion, which emerged from the former Gepoc Verfahren...
Kunststoffe international, 2014-11-26, Does Size Matter?
...rade: Purell HP570R; manufacturer: LyondellBasell Industries Basell Polyolefine GmbH in Wessling, Germany) and TPS (grade: Thermolast TM4MED; manufacturer: Kraiburg TPE) or PP (grade: Purell HP570R) and TPV (grade: Santoprene 8281-med Shore 40A; manufacturer: ExxonMobil Chemical Europe in Machelen, Belgium) exhibit a cohesive failure of the soft component only for both tested thicknesses. This is associated with force increases of 35 % and 48 % caused by the elevated cross-sectional area and a c...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.