Supernova - Purging compound - Novachem

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Supernova" in Material Data Center leads to the following information:

Tradename: Supernova
Family: Purging compound
Producer: Novachem
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2010-07-22, Thick-Walled Plastic Parts for LED Cycle Headlamps
...g process, the lenses are packaged, sent to the end customer and installed manually in the product. The cycle lamps, fully tested to road traffic licensing regulations, are now ready for use on the road. The E3 cycle lamp from Supernova contains a PMMA lens (photo: Christian Rokosch, supernova-lights.com) Fig. 1. The all-electric Elion series is characterized by reproducible mold movements, precise metering and highly precise control responses of the injection velocity and holding pressure (ph...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.