Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Sustavacu" in Material Data Center leads to the following information:

Tradename: Sustavacu
Family: PA
Producer: Gebr. Röchling KG
3 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Automobile Construction: A Substitute for Sheet Metal
...eat, as well as the low tooling cost. The company Reiss Kunststofftechnik GmbH in Tettnang/Germany manufactures various protective covers for marine engines for the firm MTU Friedrichshafen GmbH. The covers are made of the semi-finished materials Sustavacu 6 GF (Fig.1). These sheets are among the first semi-finished polyamide 6 materials for thermo-forming available on the market. They are produced by Sustaplast KG in Lahnstein/Germany and consist of durethane DP2-2140/15 Z H2.0 by Lanxess in L...

Kunststoffe international, 2005-11-21, Product Developments: Polyamides in the Engine Compartment
... polyamides has also permitted an innovative advance in thermoforming. For the very first time, extruded sheet in PA 6 is available on the market that can be processed by this method (title photo). The sheet is marketed under the brand name Sustavacu PA6 GF by Sustaplast KG in Lahnstein/Germany, which produces it from the Durethan DP2-2140/15 Z H2.0 that has already been presented. The potential savings that can be achieved by using thermoformable sheet as opposed to injection moulded parts are ...

Kunststoffe international, 2005-11-21, Strong Growth in Polyamides: Polyamide (PA)
...vative process that can be used for glass-fibre-reinforced PA6 is thermoforming. This is demonstrated by various protective covers for marine engines produced by MTU Friedrichshafen GmbH. Reiss Kunststofftechnik GmbH manufactures the covers from Sustavacu 6 GF sheets. These sheets are among the first thermoformable semi-finished products made from PA6. They consist of Durethan DP2-2140/15 Z H2.0. One of their advantages over other currently available thermoforming materials for use in marine eng...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.