Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Uvasil - Antioxidants - Addivant

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Uvasil" in Material Data Center leads to the following information:

Tradename: Uvasil
Family: Antioxidants
Producer: Addivant
2 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, HALS Light Stabiliser: Light Stabilisation and More
...iers mentioned in the text: HALS 1: Chimassorb 944 from Ciba Speciality Chemicals, Basel/Switzerland; HALS 2: Hostavin N 30 from Clariant International, Muttenz/Switzerland; HALS 3: Tinuvin 622 from Ciba Speciality Chemicals, Basel; HALS 4: Uvasil HA 88 from 3V Sigma, Bergamo/Italy) Manufacturer BASF AG G-EVP/PP – J 550 D-67056 Ludwigshafen Germany Phone +49 (0) 6 21/60-44021 Fax +49 (0) 6 21/60-6644021 www.basf.de/lightstabilizers

Kunststoffe international, 2005-11-21, One-stop Shopping
...intermediates will go on stream in the third quarter of 2001 and reach full capacity by the end of 2002. Great Lakes is currently in the process of introducing two newly developed HALS stabilizers for applications in the plastics industry. These are Uvasil 816 and 299. Uvasil 816 is a tertiary amine that provides better resistance to pesticides, for example in LDPE greenhouse sheeting. Uvasil 299 is used as a UV stabilizer for polypropylene film/sheets and additionally has an FDA (US Food and Dr...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.