Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Vistalon - EPDM - ExxonMobil Chemical Company

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Vistalon" in Material Data Center leads to the following information:

Tradename: Vistalon
Family: EPDM
Producer: ExxonMobil Chemical Company
2 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Driving the Automotive Industry: Engineering Elastomers
...0% shorter mixing cycle times. In addition to conventional EPDM co- and terpolymers, ExxonMobil, Cologne, Germany now supplies metallocene EPDM grades [2] based on Exxpol technology. Relatively new Vistalon grades with bimodal molecular weight distribution, such as Vistalon 4600 and 9500, form part of a product range expanded since K’01. They offer a good balance between the positive properties of grades with narrow molecular weight distribution (highly elastic materials) and those with wide mol...

Kunststoffe international, 2005-11-21, Elastomers
...y copolymers and terpolymers, ExxonMobil will shortly (by mid-2003) offer metallocene EPDM from the expanded plant in Baton Rouge, LA/USA, based on Exxpol technology. Modern bimodal Vistalon grades offer a combination of the good properties of grades with narrow (highly elastic materials) and broad (good processability) molecular weight distributions. They are characterised by faster and more efficient compounding, higher extruder output and, for example for blend production, significantly bette...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.