Xtel - PPS - Chevron Phillips Chemical Co

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Xtel" in Material Data Center leads to the following information:

Tradename: Xtel
Family: PPS
Producer: Chevron Phillips Chemical Co
6 hits in the material database
3 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Expanded Boundaries
...lar weight distribution and/or the addition of additives after polymerization, it was possible to overcome existing limitations and release advantageous synergies. Current examples are new PPS alloys, available with 40 % glass fibre reinforcement: - Xtel XK2040 and XK2140 grades (manufacturer: Chevron Phillips Chemicals International), which are adapted to use in the electrical engineering and electronics industries, and - Xtel XK2240 and XK2340, developed for applications in the automotive indu...

Kunststoffe international, 2005-11-21, High-performance Polymers: Metal Substitution and Miniaturisation
...onal NA, SGL Arcotec, Georg Fischer Deka and Ensinger presented a glass fibre-reinforced pipe system with pure PPS liner (Fig.2) which is immediately available in small amounts for small series. The latest PPS product form Chevron Phillips is Xtel XE3200 grade. Its low odour, freedom from halogens, high production speeds and good chemical and heat resistance make the plastic an ideal insulation material for cables and wires in vehicles, trains and ships. Under the slogan “corrosion protection u...

Kunststoffe international, 2011-10-17, Polyphenylene Sulfide (PPS)
...market. The largest of these are Fortron Industries LLC, Wilmington, NC/USA (a joint venture between Ticona Technical Polymers, Kelsterbach, Germany, and Kureha Chemical Industries Co., Ltd, Tokyo/Japan) with Fortron, Chevron Phillips with Ryton and Xtel, Toray/J&A Plastics Inc., Tokyo, with Torelina, DIC Corporation with DIC. PPS, Albis Plastic GmbH, Hamburg, Germany, with Tedur as well as Tosoh Co., Tokyo, with Petcoal. In the past few years the number of competitors, particularly in the A...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.