Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Bestdur - PBT, PET, PET+PBT - Grupo Triesa

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Bestdur" in Material Data Center leads to the following information:

Tradename: Bestdur
Family: PBT, PET, PET+PBT
Producer: Grupo Triesa
18 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
BESTDUR PH /01 PET
BESTDUR PHG3 PET-GF15
BESTDUR PHG6 PET-GF30
BESTDUR PXG3 PET-GF15
BESTDUR PXG6 PET-GF30
BESTDUR PXG7 PET-GF35
BESTDUR TH /01 PBT
BESTDUR TH /02 PBT
BESTDUR THG3 /01 PBT-GF15
BESTDUR THG4U /11 PBT-GF20
BESTDUR THG6 /01 PBT-GF30
BESTDUR THG6 /02 PBT-GF30
BESTDUR TPHG6 /01 (PBT+PET)-GF30
BESTDUR TPHG6 /02 (PBT+PET)-GF30
BESTDUR TPXG6 /02 (PBT+PET)-GF30
BESTDUR TXG4 /01 PBT-GF20
BESTDUR TXG6 /01 PBT-GF30
BESTDUR TXG6 /02 PBT-GF30

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.