Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Compadur - PBT - DimeLika Plast GmbH

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Compadur" in Material Data Center leads to the following information:

Tradename: Compadur
Family: PBT
Producer: DimeLika Plast GmbH
16 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
CompaDur® 121 GF 10 natural (003) PBT-GF10
CompaDur® 121 GF 20 natural (004) PBT-GF20
CompaDur® 121 GF 10 FR natural (011) PBT-GF10
CompaDur® 121 natural (001) PBT
CompaDur® 125GF 30 natural (016) (PBT+PET)-GF30
CompaDur® 151 natural (002) PBT
CompaDur® 121 GF 30 natural (005) PBT-GF30
CompaDur® 121 GF 20 LW natural (006) PBT-GF20
CompaDur® 121 GF 30 LW natural (007) PBT-GF30
CompaDur® 121 GK20 natural (008) PBT-GB20
CompaDur® 121 GK30 natural (009) PBT-GB30
CompaDur® 151 FR natural (010) PBT
CompaDur® 121 GF 20 FR natural (012) PBT-GF20
CompaDur® 121 GF 30 FR natural (013) PBT-GF30
CompaDur® 125GF 15 natural (014) (PBT+PET)-GF15
CompaDur® 125GF 20 natural (015) (PBT+PET)-GF20

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.