Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Lumid - PA - LG Chem

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Lumid" in Material Data Center leads to the following information:

Tradename: Lumid
Family: PA
Producer: LG Chem
62 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
LUMID EG2309B(W) PA66-GF30
LUMID GN1001AF PA6
LUMID GN1001BF PA66
LUMID GP1000B(W) PA66
LUMID GP1100A(W) PA6
LUMID GP1200A(W) PA6
LUMID GP1300A(W) PA6
LUMID GP1300AP PA6
LUMID GP2101BF PA66-GF10
LUMID GP2130A(W) PA6-GF13
LUMID GP2130AE PA6-GF13
LUMID GP2130B(W) PA66-GF13
LUMID GP2151AF PA6-GF15
LUMID GP2200A(W) PA6-GF20
LUMID GP2200B(W) PA66-GF20
LUMID GP2251BF PA66-GF25
LUMID GP2259AFL PA6-GF25
LUMID GP2300A(W) PA6-GF30
LUMID GP2301BF PA66-GF30
LUMID GP2309A(W) PA6-GF30
LUMID GP2330A(W) PA6-GF33
LUMID GP2330B(W) PA66-GF33
LUMID GP2330BL PA66-GF33
LUMID GP2339B(W) PA66-GF33
LUMID GP2430A(W) PA6-GF43
LUMID GP2430B(W) PA66-GF43
LUMID GP2500A(W) PA6-GF50
LUMID GP2500B(W) PA66-GF50
LUMID GP3150A(W) PA6-MF15
LUMID GP3200A(W) PA6-MF20
LUMID GP3200B(W) PA66-MF20
LUMID GP3300A(W) PA6-MF30
LUMID GP3300B(W) PA66-MF30
LUMID GP3400A(W) PA6-MF40
LUMID GP3400B(W) PA66-MF40
LUMID HI1102A(W) PA6
LUMID HI1102B(W) PA66
LUMID HI1202A(W) PA6
LUMID HI1202B(W) PA66
LUMID HI2152A(W) PA6-GF15
LUMID HI2202B(W) PA66-GF20
LUMID HI2302A(W) PA6-GF30
LUMID HI3232A(W) PA6-MF23
LUMID HI5001AH (PA6+EPDM+PE-HD)
LUMID HI5001AS (PA6+EPDM+PE-LD)
LUMID HI5003A (PA6+EPDM+PP)
LUMID HI5006A(W) (PA6+ABS)
LUMID HI5063A(W) (PA6+ABS)-MF6
LUMID HI5083A(W) (PA6+ABS)-MF8
LUMID LW4203A(W) PA6-(GF+MF)20
LUMID LW4303B(W) PA66-MF30
LUMID LW4403A(W) PA6-(GF+MF)40
LUMID LW4409A(K) PA6-(GF+MF)40
LUMID SG2300B(W) PA66-GF30
LUMID SG2460B PA66-GF46
LUMID SG2600B PA66-GF60
LUMID SG4389B PA66-(GF+MF)38
LUMID GN2251BF PA66-GF25
LUMID GP2150A(W) PA6-GF15
LUMID HM2604A(W) PA6-GF60
LUMID GP2300BW PA66-GF30
LUMID HI5006A (PA6+ABS)

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.