Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Schulamid - PA12, PA6, PA612, PA66 - LyondellBasell Industries

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Schulamid" in Material Data Center leads to the following information:

Tradename: Schulamid
Family: PA12, PA6, PA612, PA66
Producer: LyondellBasell Industries
156 hits in the material database
7 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
SCHULAMID® 6 GB 15 LS PA6-GB15
SCHULAMID® 6 GB 30 PA6-GB30
SCHULAMID® 6 GB 30 LS PA6-GB30
SCHULAMID® 6 GBF 3010 H PA6-(GB+GF)30
SCHULAMID® 6 GBF 3015 FR 4 PA6-(GB+GF)30
SCHULAMID® 6 GBF 3026 H LW PA6-(GB+GF)30
SCHULAMID® 6 GF 15 PA6-GF15
SCHULAMID® 6 GF 15 FR 4 K1681 PA6-GF15 FR(17+30)
SCHULAMID® 6 GF 15 H PA6-GF15
SCHULAMID® 6 GF 15 HI PA6-I-GF15
SCHULAMID® 6 GF 15 HI BM PA6-I-GF15
SCHULAMID® 6 GF 15 HI K2073 PA6-I-GF15
SCHULAMID® 6 GF 15 HV PA6-GF15
SCHULAMID® 6 GF 15 UV PA6-GF15
SCHULAMID® 6 GF 20 H PA6-GF20
SCHULAMID® 6 GF 20 H LS PA6-I-GF20
SCHULAMID® 6 GF 25 PA6-GF25
SCHULAMID® 6 GF 25 FR PA6-GF25
SCHULAMID® 6 GF 30 PA6-GF31
SCHULAMID® 6 GF 30 FR 2 PA6-GF30
SCHULAMID® 6 GF 30 FR 4 PA6-GF30 FR
SCHULAMID® 6 GF 30 GID LS PA6-GF30
SCHULAMID® 6 GF 30 GID natur PA6-GF30
SCHULAMID® 6 GF 30 H PA6-GF30
SCHULAMID® 6 GF 30 H BLACK REC PA6-GF30
SCHULAMID® 6 GF 30 H LW PA6-GF30
SCHULAMID® 6 GF 30 HI PA6-GF30
SCHULAMID® 6 GF 30 HI K1871 PA6-GF30
SCHULAMID® 6 GF 30 HI WIT PA6-GF30
SCHULAMID® 6 GF 30 TC PA6-I-GF30
SCHULAMID® 6 GF 33 PA6-GF33
SCHULAMID® 6 GF 33 RN PA6-GF33
SCHULAMID® 6 GF 34 HI PA6-GF34
SCHULAMID® 6 GF 35 PA6-GF35
SCHULAMID® 6 GF 35 H BLACK REC PA6-GF35
SCHULAMID® 6 GF 40 PA6-GF40
SCHULAMID® 6 GF 43 RN PA6-GF43
SCHULAMID® 6 GF 45 H PA6-GF45
SCHULAMID® 6 GF 50 PA6-GF50
SCHULAMID® 6 GF 50 TSU PA6-GF50
SCHULAMID® 6 HV 0 H FR PA6
SCHULAMID® 6 HV 11 PA6
SCHULAMID® 6 HV 15 PA6
SCHULAMID® 6 HV 2 FR PA6
SCHULAMID® 6 LV 12 PA6
SCHULAMID® 6 MGF 45 FR 6 PA6-(GF+MX)45
SCHULAMID® 6 MKF 3010 H PA6-(GF+MD)30
SCHULAMID® 6 MKF 3010 HI PA6-(GF+MD)30
SCHULAMID® 6 MKF 4014 PA6
SCHULAMID® 6 MKF 4015 PA6-(GF+MD)40
SCHULAMID® 6 MKF 4520 H PA6-(GF+MD)45
SCHULAMID® 6 MT 25 FR PA6-MX25
SCHULAMID® 6 MT 30 PA6-T30
SCHULAMID® 6 MV 13 PA6
SCHULAMID® 6 MV 14 PA6
SCHULAMID® 6 MV 14 FR PA6 FR
SCHULAMID® 6 MV 14 FR 4 K1681 PA6
SCHULAMID® 6 MV 5 PA6
SCHULAMID® 6 MV HI PA6-I
SCHULAMID® 6 MV HI K1893 PA6-I
SCHULAMID® 6 MV SHI PA6-I
SCHULAMID® 6 NV 12 PA6
SCHULAMID® 6 NV 12 FR PA6 FR(17)
SCHULAMID® 612 FS 4003 PA612
SCHULAMID® 612 FS 4004 PA612
SCHULAMID® 612 FS 4104 PA612
SCHULAMID® 612 GF 30 HI PA612-GF30
SCHULAMID® 612 IC 4005 W PA612
SCHULAMID® 66 CF 20 H PA66-CF20
SCHULAMID® 66 GB 30 PA66-GB30
SCHULAMID® 66 GB 30 H PA66-GB30
SCHULAMID® 66 GB 40 PA66-GB40
SCHULAMID® 66 GBF 3020 PA66-(GB+GF)30
SCHULAMID® 66 GBF 3020 FR 4 PA66-(GB+GF)30
SCHULAMID® 66 GF 13 PA66-GF13
SCHULAMID® 66 GF 13 HI UV PA66-GF13
SCHULAMID® 66 GF 15 H PA66-GF15
SCHULAMID® 66 GF 15 HI H PA66-I-GF15
SCHULAMID® 66 GF 15 HI K2034 PA66-GF15
SCHULAMID® 66 GF 25 EGR PA66-GF25
SCHULAMID® 66 GF 25 FR 5 A PA66-GF25
SCHULAMID® 66 GF 25 H PA66-GF25
SCHULAMID® 66 GF 30 PA66-GF30
SCHULAMID® 66 GF 30 FR 2 PA66-GF30
SCHULAMID® 66 GF 30 GID PA66-GF30
SCHULAMID® 66 GF 30 GID K1802 PA66-GF30
SCHULAMID® 66 GF 30 H PA66-GF30
SCHULAMID® 66 GF 30 H BLACK REC PA66-GF30
SCHULAMID® 66 GF 30 HE LW PA66-GF30
SCHULAMID® 66 GF 30 HI PA66-GF30
SCHULAMID® 66 GF 30 HR PA66-GF30
SCHULAMID® 66 GF 33 PA66-GF33
SCHULAMID® 66 GF 33 H PA66-GF33
SCHULAMID® 66 GF 33 HS PA66-GF33
SCHULAMID® 66 GF 35 PA66-GF35
SCHULAMID® 66 GF 35 H PA66-GF35
SCHULAMID® 66 GF 35 H BLACK REC PA66-GF35
SCHULAMID® 66 GF 35 HE GREY 967826 PA66-GF35
SCHULAMID® 66 GF 40 H PA66-GF40
SCHULAMID® 66 GF 43 H PA66-GF43
SCHULAMID® 66 GF 43 RN PA66-GF43
SCHULAMID® 66 GF 50 H PA66-GF50
SCHULAMID® 66 GRF 2318 H PA66-(GF+CD)23
SCHULAMID® 66 MF 20 PA66-MD20
SCHULAMID® 66 MF 40 PA66-MX40
SCHULAMID® 66 MK 30 HI PA66-MX30
SCHULAMID® 66 MK 30 HI H K1357 PA66-I-MX40
SCHULAMID® 66 MK 4015 H PA66-(GF+MD)40
SCHULAMID® 66 MKF 40 HI PA66-MD40
SCHULAMID® 66 MKF 4015 PA66-(GF+MD)40
SCHULAMID® 66 MNF 2510 H PA66-(GF+MX)25
SCHULAMID® 66 MV 2 PA66
SCHULAMID® 66 MV 3 HI PA66
SCHULAMID® 66 MV HI PA66
SCHULAMID® 66 MV HI H K1416 PA66
SCHULAMID® 66 MV HI HH K2300 PA66
SCHULAMID® 66 MV HI K1416 PA66
SCHULAMID® 66 MW 30 FR 4 PA66-MD30
SCHULAMID® 66 MW 30 FR 4 K2031 PA66-MX30
SCHULAMID® 66 PTFE 20 HS PA66
SCHULAMID® 66 SK 1000 PA66
SCHULAMID® 66/6 GF 33 H PA666-GF33
SCHULAMID® 66/6 MT 20 K1849 (PA666+PA66)-T20
SCHULAMID® B 6 MKF 4015 PA6-(GF+MX)40
SCHULAMID® E-17222 PA66
SCHULAMID® 6 GBF 3015 FR 2 PA6-(GB+GF)30
SCHULAMID® 6 GBF 3020 K1697 PA6-(GB+GF)30
SCHULAMID® 6 GBF 3310 HI H LS PA6-(GB+GF)33
SCHULAMID® 6 GF 15 H K1432 PA6-GF15
SCHULAMID® 6 GF 15 SHI K2384 PA6-GF15
SCHULAMID® 6 GF 20 FR NATURAL PA6-GF20 FR(30)
SCHULAMID® 6 GF 7 FR 4 K1681 PA6-GF7 FR(17+30)
SCHULAMID® 6 MKF 4015 K2098 PA6-(GF+MD)40
SCHULAMID® 6 MV 13 F PA6
SCHULAMID® 6 RBL 3000 BLACK PA6-GF30
SCHULAMID® 612 FS 5003 MC PA612
SCHULAMID® 612 GF 30 H PA612-GF30
SCHULAMID® 612 GF 30 H9 PA612-GF30
SCHULAMID® 612 GF 33 HE PA612-GF33
SCHULAMID® 612 GF 50 H PA612-GF50
SCHULAMID® 612 GF 65 H IS PA612-GF65
SCHULAMID® 612 HV H 5003 PA612
SCHULAMID® 66 GF 25 PA66-GF25
SCHULAMID® 66 GF 30 FC PA66-GF30
SCHULAMID® 66 GF 30 HE PA66-GF30
SCHULAMID® 66 GF 33 RN PA66-GF36
SCHULAMID® 66 GF 35 FC4 PA66-GF35
SCHULAMID® 66 GF 43 HRN PA66-GF43
SCHULAMID® 66 MV 5 FR PA66 FR(30)
SCHULAMID® 66 MV HI H2 PA66
SCHULAMID® 66 MV HI20 PA66
SCHULAMID® 66 RBL 2500 BLACK PA66-GF25
SCHULAMID® RD 6 GF 30 PA6-I-GF30
SCHULAMID® XM GF 50 BLACK (PA66+PA6I/6T)-GF50
SCHULAMID® XM GF 60 BLACK (PA66+PA6I/6T)-GF60
SCHULAMID® XT 200 GF 50 NATURAL PA66-GF50

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.