Material datasheets available free. Online registration at: www.materialdatacenter.com
Triax - ABS+PA - INEOS Styrolution
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Triax" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...roducts from four manufacturers are significant on the market (Table 2). Blends with PC include Terblend S (BASF), Bayblend (Bayer), Pulse (Dow) and Cycoloy and Geloy (GE Plastics). (PA+ABS) blends are marketed by BASF as Terblend N and by Bayer as Triax. Market Segments Thanks to their versatile applications and processing properties, styrene copolymers have been able to compete very effectively with other engineering thermoplastics and commodities in recent years. For example, styrene copoly...
Kunststoffe international, 2005-11-30, Retrofit on a Milling Machine: 19 Years’ Service and Better than New
...ant management had to decide whether to carry out a general overhaul of the machine, which was nearly 20 years old, or purchase a new unit. Reinhold Kuchenmeister Since 1986, Poly Hi Solidur Deutschland GmbH, Vreden/Germany, has been using the NC Triax 2 T CMS milling machine (manufacturer: C.M.S. S.p.A., Zogno/Italy) to machine engineering plastics. After many years’ intensive service, machine failure was imminent. Josef Willemsen, the production manager, was faced with the problem of safeguar...
Kunststoffe international, 2007-03-15, More Lightweight Construction for the BMW 3 Series Coupé and Convertible Models
...perational reasons a material was selected which in comparison with the side panel of the BMW 6 series exhibits other decisive advantages in addition to online paintability. The material selected, a mineral-filled blend of PA and ABS (grade: Triax DP 3157) from the Lanxess company, Leverkusen/Germany, is characterised by a lower coefficient of thermal expansion than the (PA+PPO) blend. In addition, the additive present in the material significantly reduces moisture absorption and especially the ...
Kunststoffe international, 2007-08-14, Goal: Quicker Return on Investment
... seen to represent an important future market, especially in the field of mechatronics. The styrene copolymers from Lustran Polymers contribute to economical and high-quality surfaces for plastic components in the future. For instance, Triax DP 3157, the online-paintable polyamide+ABS blend is already employed in a project with BMW for body components with class A surfaces. New ABS and ASA resins could provide soft-touch surfaces via coextrusion or lamination, for instance, for vehicle interiors...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.