Material datasheets available free. Online registration at: www.materialdatacenter.com
Schulamid - PA12, PA6, PA612, PA66 - LyondellBasell Industries
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Schulamid" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...nes (Fig.1). A. Schulmann is also supplying a special material combination for water-assist technology. Two-component injection moulding in combination with water-assist technology is used to produce cooling water pipes. The outer skin is made from Schulamid 66 GF30 2K WIT, while on the inside Polyfort FPP FX2020 E ensures easy processability with water and good internal surface quality. In the halogen-free sector, Lanxess is launching new PA6 and PA66 grades. The PA6 materials are the Durethan...
Kunststoffe international, 2005-11-21, Flame Retardants: Growing Demand
... halogen-free UL94 V0 polypropylene compound with a very good Shore hardness. A. Schulman GmbH presented different flame-retarded compounds for polypropylene, polyamide, polybutylene terephthalate and (PC+ABS). The special feature of Schulamid NV 12FR – a polyamide 6 without halogen or red phosphorous – is that it attains a UL94 V0 rating, a GWFI of 960°C and a GWIT of 750°C in a thickness of 0.4 to 3.0mm. Polyflam RIPP 490 is a halogen-free polypropylene which, in a thickness of 1.5mm, attains ...
Kunststoffe international, 2008-02-17, Few New Products but Business is Booming
...s in the 1.0 to 1.8mm size range. The advantages of these are dust-free processing and an optimal dispersion in the polymer melt. A. Schulman, Kerpen, Germany, presented flame retardant compounds for the automobile industry. Schulamid 66 GBF3020 FR4, a flame retarded polyamide 66, is UL94 V0 listed and is used for the manufacture of control unit casings for electrical systems. The polyamide housings have complex geometries and a tendency to warp. A specially balanced mix of glass spheres and gla...
Kunststoffe international, 2008-02-29, Louvers Reduce Fuel Consumption
... choice of injection molding parameters. In addition to the general process parameters, material selection represented one further important factor. The rigid carrier for the louvers is molded from glass fiber reinforced polyamide 6 (PA6; grade: Schulamid GF 30 H, supplier: A. Schulman GmbH), the flexible lips from the thermoplastic elastomer (TPS) (grade: Thermolast TC6PAZ-C200, supplier: Kraiburg TPE GmbH). The housing is molded from glass fiber reinforced polypropylene (grade: Polyfort PP GF ...
Kunststoffe international, 2009-10-14, Race of Products
...many, took 1st place for the component in the ''''Automotive body exterior category at the Automotive Awards presented by the Society of Plastic Engineers (SPE). The grille is manufactured from a silver-metallic, high-impact polyamide (Schulamid 66 MT5 HI LS). This material permits production of a visually appealing, high-quality radiator grille in only one step; painting is eliminated. Production costs are reduced and the utilitarian value increased. Flow and weld lines present a challenge wh...
Kunststoffe international, 2018-03-09, Strong Flyweights
...d vehicle from one of the German automobile manufacturers (Fig. 1). The part measures 255 mm x 270 mm and has a wall thickness ranging from 1.5 to 2.5 mm. The previous version weighed 148 g and consisted of the glass fiber-reinforced polyamide (PA) Schulamid 6 GF30. Its materials properties, dimensional stability, and shrinkage, in particular, were to be approximated in a newly developed lighter plastic.Obtaining a lower-density polyamide by blending it with lighter polymers has been no problem ...
Kunststoffe international, 2018-05-15, Power Lies in the Water
...e to be generated in the region of greatest cross-sectional area. In addition, with the use of the short shot process, a flow mark is very likely to be produced at the point of partial filling.The PA6 with 30 % glass fibers used (type: Schulamid 6 GF 30 HI WAIM; manufacturer: A. Schulman) was developed for general use in WAIM. The handles are produced in several hydraulic injection molding machines (type: Victory 180, manufacturer: Engel Austria GmbH) in a cycle time of approx. 52 s. Subsequentl...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.