Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Bakelite - EP, MPF, PF, UP - Bakelite Synthetics

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Bakelite" in Material Data Center leads to the following information:

Tradename: Bakelite
Family: EP, MPF, PF, UP
Producer: Bakelite Synthetics
60 hits in the material database
15 hits in the literature database
36 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Application
Bakelite® EP 8412 Magnetic coils
Bakelite® MP 4165 Commutators for lifters and servo motors
Bakelite® PF 2535 Pot grips and handles
Bakelite® PF 2560 Oven grips
Bakelite® PF 2736 Coil bodies
Bakelite® PF 2736 PTCs (temperature-dependent resistors)
Bakelite® PF 2774 Power switches (arc chamber)
Bakelite® PF Motor overload relay
Bakelite® PF 2874 Carbon brush holders
Bakelite® PF 2874 Switch covers
Bakelite® PF 2874 Drive elements (dual-belt pulleys)
Bakelite® PF 31 Switching housings and rotary switches
Bakelite® PF 31 Pot grips and handles
Bakelite® PF 31 Lamp sockets
Bakelite® PF 4109 Commutators for industrial motors
Bakelite® PF 4155 Commutators for household appliances
Bakelite® PF 6501 Pulleys
Bakelite® PF 6507 Water pump bodies
Bakelite® PF 7592 Oven trim, chrome plated
Bakelite® PF 7595 Vacuum pump
Bakelite® PF 7595 Gas meters (valve functional elements)
Bakelite® PF 8052 Pot grips and handles
Bakelite® PF 51 Power switches (insulator)
Keripol RW 1411 Lamp bases
Bakelite® UP 3415 Power switches (arc chamber)
Bakelite® UP 3415 Motor overload relay
Bakelite® UP 3415 Energy regulator housings
Bakelite® UP 3415 Circuit breakers for equipment (functional element)
Bakelite® UP Coil bodies
Bakelite® UP 3620 Power switches (arc chamber)
Bakelite® UP 3720 Power switches (insulator)
Bakelite® UP 802 Distributor caps, rotors
Bakelite® UP 802 Sparkplug caps
Bakelite® UP 804 Power circuit breakers (for high switching currents)
Bakelite® UP 804 Oven grips
Bakelite® X 22 Lamp sockets

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.